Abstract

In this study, off-axis magnetron sputtering was used for the crystallized ITO thin films at a low temperature of about instead of the conventional RF sputtering because the off-axis sputtering can avoid the damage for the plasma as well as fabrication of thin films with a high quality. The ITO thin films grown on PET substrate at were crystallized with a (222) preferred orientation. 58-nm thick ITO films showed a resistivity of about and a transmittance of about 75% at a wavelength of 550 nm. The transmittance of the ITO thin films by an insertion of SiO2 thin films on ITO films was improved.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.