Abstract

The short-transverse fracture toughness behavior of aluminum-lithium alloy 8090 plate was investigated by using a CNSB (chevron notched short bar) specimen. The fracture toughness KQVM was reduced with a progress of the first-step aging. The double-aged (DA) alloy, which was subjected to the initial underaging (UA2) at 433K followed by the second-step aging at a higher temperature for a short time, exhibited a fairly improved KQVM and a superior strength-toughness balance in comparison with the single-aged alloy, good enough to satisfy the toughness requirement in aircraft design, KQVM/σys≥2.5√mm, where σys is yield strength. The increase in toughness by DA treatment is attributed to the relaxation of intense slips due to dissolution of shearable δ' phase and growth of δ'-PFZ width, leading to the inhibition of intergranular fracture.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.