The effect of the modifying additive ZrO2 on the rheological properties, the processes of structure and phase formation of the compositions of the Y2O3–Al2O3–SiO2 system obtained by the sol-gel method has been investigated. It was found that the temperature range of crystallization of the compositions of the Y2O3–Al2O3–SiO2 system with the addition of ZrO2 is 1020–1270 °C and with an increase in the concentration of zirconium oxide, the amount of the main crystalline phase of yttrium pyrosilicate (β-Y2Si2O7) decreases and the concentration of the zirconium-containing phase – the tetragonal modification of zirconium oxide and zirconium silicate ZrSiO4 -increases.