For production of case furniture wood-shaving plates (DSTP) and medium-density fiber boards - plates of the PMV wood monostructural fibrous brand (plate MDF) are widely used. And, both faces, and edges of plates come to production of furniture the revetted thermosetting polymeric films, sliced veneer or other cladding materials, for example paper-based laminated plastic (BSP). 
 One of the main defects of such plates is the insufficient durability of their outside or surface layers of face that is one of shortcomings of plates as leads to flaking of cladding material. And, when flaking the facing layer entrains part of surface layer of plate. Indicator of durability of skin of plates is the specific resistance to normal separation of layer at depth of 0,3 - 0,7 mm from plate surface which is defined in accordance with GOST 23234-2009 [1].
 However, as have shown results of our researches, in a number of standards on wood processing it is necessary to make changes in part of test method of plates on the specific resistance to normal separation of layer of skin not at depth of 0,3 - 0,7 mm (as in accordance with GOST 23234-2009), and surface layer. In this regard it is necessary to make changes to state standard specifications 10632-2014 [2] and 32274-2013 [3] on required values of specific resistance to normal separation of surface layer, but not layer at depth of 0,3 - 0,7 mm from plate surface.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.