Abstract

Abstract The frequency dependences of the dissipation factor tanδ( f ) and the Cole–Cole diagrams for germanium- and magnesium-doped vanadium-dioxide films in the range of 0.1–10^6 Hz are obtained. Measurements at temperatures between 173–373 K are performed. It is found that, at room temperature, an additional maximum in the tanδ( f ) dependence and an additional semicircle in the Cole–Cole diagram of the VO_2:Ge films as compared with those of undoped films appear at low frequencies. In the VO_2:Mg films, similar additional features in the dielectric spectra are observed at high frequencies. It is shown that the shape of the Cole – Cole diagrams for all the films is almost temperature independent in the mentioned temperature range, while the frequencies f _0 corresponding to the tanδ( f ) maxima increase with temperature. To interpret the dielectric spectroscopy data, a combined equivalent electrical circuit of the film sample is proposed. The mechanisms of the effect of Ge and Mg impurities on the characteristics of the complex Mott–Peierls semiconductor–metal phase transition are established.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.