To evaluate relevant material properties (flexural strength [σf], elastic modulus [E], water sorption [Wsp] and solubility [Wsl], and biocompatibility) of an additive manufacturing (AM) polymer vs a heat-curing acrylic resin (AR; control) for the manufacture of complete dentures, testing the hypothesis that fabrications from both materials would present acceptable material properties for clinical use. The σf, E, Wsp, and Wsl were evaluated according to the ISO 20795-1:2013 standard, and the biocompatibility was evaluated using MTT and SRB assays. Disk-shaped specimens were fabricated and used for Wsp (n = 5), Wsl (n = 5), and biocompatibility (n = 3) testing. For assessment of σf and E, bar-shaped specimens (n = 30) were fabricated and stored in 37°C distilled water for 48 hours or 6 months before flexural testing in a universal testing machine with a constant displacement rate (5 ± 1 mm/minute). Data from σf, E, Wsp, Wsl, and biocompatibility tests were statistically analyzed using Student t test (α = .05). Weibull analysis was also used for σf and E data. Significant differences between the two materials were found for the evaluated material properties. Water storage for 6 months did not affect the flexural strength of the AM polymer, but this material showed inadequate σf and Wsl values. Despite adequate biocompatibility and strength stability after 6 months of water storage, the AM polymer recommended for complete dentures needs further development to improve the material properties evaluated in this study.
Read full abstract