Background: Adhesive strength is one of the most important properties of the hardened mortar, and influenced by mortar workability (i.e. mortar water content), and substrate roughness surface degree. Objective: This study aims to measure the adhesion strength between three different hydrated aerial lime mortars, and the two most common building units in old and modern building in Loire valley in France: Tuffeau and Siporex, under different relative humidity (12,66,98%) and curing periods (7,28,90 days). Materials and Methods: These mortars include: B/F (1:5.6: Moisture=46 %, aggregate stone powder pass sieve NO.2mm), B/W (1:5.6: Moisture=44 %, aggregate stone powder pass sieveNO.2mm and retained on sieve NO. 0.16mm), and B/F/M (1:5.6: Moisture=35%: superplasticizer water reducer Melment F10 (2.5% of lime amount), aggregate stone powder pass sieve NO.2mm). Numerous complementary techniques have been used to achieve this study, such as: x-ray diffraction, coupled plasma optical emission spectrometry, mercury intrusion porosimetry, mortars axial expansion by consolidation apparatus, and Proceq-DY-215 apparatus for adhesive strength measurement. Results: The results showed that expansion of B/F, B/W, and B/F/M has little effect on their adhesion strength with Tuffeau /Siporex substrates. Also, the adopted relative humidity variations had a limited effect on the adhesion strength of B/W along the curing periods (7, 28, and 90 days), with noticeable effect for the other mortars. Conclusions: The conclusions referred to the important impact of the degree of substrate surface roughness on the adhesive strength of all used mortars, where the use of Siporex as substrate recorded a clear advantage compared to Tuffeau under all used relative humidity and curing periods.
Read full abstract