Abstract
Lithium ion battery (LIB) is widely used energy storage device. Herein, we report the preparation of ZnWO4/SnO2 nanocomposite and ZnWO4/SnO2@r-GO nanocomposite via solvothermal method. The structural, elemental and morphological properties of the prepared samples are characterized using x-ray diffraction (XRD), scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDAX), high-resolution transmission electron microscopy (HR-TEM), Brunauer-Emmett-Teller (BET) measurements, Raman spectroscopy and X-ray photoelectron spectroscopy (XPS) techniques. The prepared samples are tested as an anode for LIB. The ZnWO4/SnO2 (5%) nanocomposite delivers initial discharge capacity of 882 mAh g−1 at a current density of 100 mA g−1, while, the specific capacity increases with the increase of SnO2 upto 10% tested in present case. Further, ZnWO4/SnO2@r-GO nanocomposite exhibits a discharge capacity of 1486 mAh g−1 which is higher than that of ZnWO4/SnO2 nanocomposite. In addition, after 500 cycles ZnWO4/SnO2@r-GO nanocomposite exhibits 89.8% cycle life and 98% of discharge capacity retention. These results indicate that, ZnWO4/SnO2@r-GO nanocomposite is a promising anode material for LIB.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.