The slurry erosion behavior of a zirconium based bulk metallic glass, Zr44Ti11Cu10Ni10Be25, was evaluated in this study. Slurry erosion tests were carried out using a non-circulating type test rig at impingement angles of 30°, 60°, and 90°. Commonly used hydroturbine steel was evaluated under the same test conditions. At 30° impingement angle, the metallic glass demonstrated nearly 2.6 times higher erosion resistance compared to the steel. At normal impingement, the metallic glass was marginally better. Lower erosion rates of the bulk metallic glass at oblique impingement angles was attributed to its significantly higher hardness and deformation induced partial devitrification. For normal impingement, material was removed in the form of fragments from highly strained platelets due to limited plasticity of bulk metallic glasses. The metallic glass demonstrated a brittle mode of erosion with higher erosion rate at higher angle of impingement. In contrast, hydroturbine steel showed ductile mode of erosion under the same test conditions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.