Abstract The results of an investigation on slip cast and sintered Y 2 O 3 (3 wt%)- stabilized ZrO 2 with additions of 5, 10, 15 wt% Al 2 O 3 are reported. The surface roughness, porosity and density of the samples were measured. The hardness HRc and Hv, fracture toughness K 1C , and friction coefficients were also measured using standard methods. The structural properties of the samples were observed by Scanning Electron Microscopy (SEM). The surface topography was evaluated by means of Chromatic White Light Interferometry using MicroSpy® Topo of FRT Rauheit Kontur before and after tribological tests. The phase and chemical composition were analyzed by X-Ray Diffractometry (XRD), Energy Dispersive X-ray (EDX) spectroscopy, and Raman spectroscopy. Results show that the addition of Al 2 O 3 into YSZ ceramics in the range of 5–10% allows the mechanical and tribological characteristics of the material that can be applied in different mechanical machines for different metallurgical processes to be improved, as well as in chemical engineering or medicine.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.