Mechanical properties of bulk ZnO single crystals are studied depending on crystallographic orientation, temperature and radiation. The shapes of the indenter prints and dislocation rosettes were analyzed for the faces of monohedron (0001), hexagonal prisms {1010}, {11 20}, and pyramid {1011}. For {1010} plane, the fracture toughness coefficient K 1C was found to be K 1C ∼0.09 MPa m 1/2 , Young modulus E = 47.7 GPa, microhardness H = 1.7 GPa, coefficient of surface energy of destruction y = 0.085 J/m 2 . For (0001) face H = 4.2 GPa.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.