Abstract
ABSTRACTThe yield strength anomaly (YSA) and dynamic strain ageing (DSA) behaviour of advanced ultra-supercritical boiler grade wrought nickel-based superalloy IN 740H is studied by conducting tensile tests in temperature range 28–930°C and by employing strain rates 1 × 10−2, 1 × 10−3, 1 × 10−4 and 1 × 10−5 s−1 followed by extensive electron microscopic examination. Increase in yield strength accompanied by impairment of ductility indicates that YSA exists in alloy IN 740H in temperature range of 650–760°C. The electron microscopic observation confirms that YSA is due to pinning of dislocations by γ′ precipitates and shearing of γ′ precipitates in IN 740H. DSA is observed in the temperature range of 200–500°C and is predominant at 300°C. The nature of serrated plastic flow due to DSA is dependent on the temperature and strain rate.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.