Abstract
We tried to apply the nanoindentation technique to yield strength characterization by modifying a previous research. Although the yield strength determining technique developed by Kramer et al. has been successfully demonstrated for large scale indentations on bulky metals, its applicability is still doubtful to nanoscale indentations on thin films with severe roughness, anisotropy, and interfacial constraint. In order to overcome these problems, we combined the nanoindentation technique with a three-dimensional indent visualization technique in this study. Nanoindentation tests were performed for Au and TiN thin films and their corresponding indents were scanned by using an atomic force microscope. From the three-dimensional pile-up morphology, a circular pile-up boundary was measured and input into the yield strength formulation as an effective yielded zone radius. The yield strengths calculated were directly compared with those from the microtensile test.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.