Abstract
Differential deposition by DC magnetron sputtering was applied to correct for figure errors of X-ray mirrors to be deployed on low-emittance synchrotron beamlines. During the deposition process, the mirrors were moved in front of a beam-defining aperture and the required velocity profile was calculated using a deconvolution algorithm. The surface figure was characterized using conventional off-line visible-light metrology instrumentation (long trace profiler and Fizeau interferometer) before and after the deposition. WSi2 was revealed to be a promising candidate material since it conserves the initial substrate surface roughness and limits the film stress to acceptable levels. On a 300 mm-long flat Si mirror the average height errors were reduced by a factor of 20 down to 0.2 nm root mean square. This result shows the suitability of WSi2 for differential deposition. Potential promising applications include the upgrade of affordable, average-quality substrates to the standards of modern synchrotron beamlines.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.