Abstract
AbstractAn XRD method for measurement of quartz content using ZnO as the internal standard was tested on different particle sizes between 0 and 20µm. Calibration curves showed a good correlation coefficient for particle-size fractions up to 20µm; the slope increased for the fractions from 0·7 to 5µm and was relatively constant for coarser particle sizes. Fine quartz fractions were etched with hydrofluoric acid to remove the surface layer damaged during dry grinding. The use of such etched quartz increased the slopes of the calibration curves for small particle-size fractions and approximated the natural fine quartz fraction much better than the original dry-ground material. The mean of six measurements gave good accuracy provided that the slope of the calibration curve was adjusted for the particular particle-size fraction. This method was used on 0–2µm, 0–0·2µm and 0·2–2µm fractions of French silty soils and the results are in agreement with the data from chemical analysis and with the mineralogical interpretation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.