Abstract The Y2O3:Er3+/Yb3+ crystal fiber material has been successfully prepared by laser heated pedestal growth method. The X-ray diffraction results indicate that the prepared Y2O3:Er3+/Yb3+ luminescent material, which is optically transparent under the optical microscope, possesses pure Y2O3 crystal phase. The up-conversion luminescence corresponding to the (2H11/2, 4S3/2, 4F9/2) → 4I15/2 transitions of Er3+ ions were recorded under a 976 nm laser diode excitation. The up-conversion emission intensities from the 2H11/2 → 4I15/2 and 4S3/2 → 4I15/2 transitions of Er3+ ions were studied from room temperature to 873 K by fluorescence intensity ratio (FIR) technique. It has been found that the prepared Y2O3:Er3+/Yb3+ crystal fiber has high-efficient up-conversion emissions, and effectively improves the temperature measurement accuracy and range, making Y2O3:Er3+/Yb3+ crystal fiber an interesting candidate for optical temperature sensor.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.