Abstract

We used a validated femoral resurfacing model to obtain measurements of pressure and temperature and quantify cement distribution as a function of inner geometry and cementing technique of five different femoral hip resurfacing components. The purpose was to investigate if manufacture cementing recommendations are reliable. ASR showed only with the recommended manual cementing technique low cement pressures of 58.0±50.2kPa and low interface temperatures of 33.3±4.1°C. BHR had large cement defects of 10.4±1.1mm. Conserve Plus caused the smallest cement penetration depths of 2.9±0.6mm. Durom was tolerant against changes of the cementing technique but showed the widest spread of temperature data 42.8±7.0°C. ReCap showed the highest risk for incomplete seating with a cement mantle thickness of 4.3±0.9mm. Polymerization heat did not exceed the threshold of 45°C with a cement penetration depth of less than 4.2mm in any circumstances of this study.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.