Abstract
In this work, well-dispersed fumed SiO2/cis-1,4-polyisoprene rubber (IR) masterbatch was first obtained through an effective wet mixing method, and the properties of the corresponding vulcanizate were studied. Before curing with activator and sulfur, IR solution was blended and co-coagulated with SiO2 suspension modified by bis(3-trimethoxysilypropyl) tetrasulfide in n-hexane. The modification of TESPT imparted evenly distributed SiO2 particles in IR and improved interfacial binding among SiO2 and IR. Hence, the prepared compound presented better processability and the corresponding vulcanizate presented higher physical performance, including higher tensile strength, lower heat buildup, and better fatigue resistance than that prepared in the dry mixing method. Additionally, higher wet skid resistance and lower rolling resistance could be observed in fabricated SiO2/IR vulcanizate. The employed wet mixing method is economical and efficient, which is promising in preparing rubber composites with comprehensive performance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.