Abstract

This paper presents an experimental study on resistance spot welding of SPA-C steel sheets used in rail vehicles. SPA-C steel sheets having 2.3 mm thicknesses were joined by using resistance spot welding as lap joint. A timer and current controlled resistance spot welding machine having 120 kVA capacity and a pneumatic application mechanism with a single lever was used to prepare the specimens. Welding periods were chosen as 5, 10, 15, 20, 25 and 30 cycles and also welding currents were increased from 6 kA up to 14 kA by rise of 0,5 kA. The electrode force was kept constant at 6 kN. The obtained welding joints were exposed to tensile-peel and tensile-shear tests. Welding time effect on tensile-peel strength and tensile-shear strength were researched by using related diagrams and the optimum welding currents and times were advised.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.