Petroleum refineries and power plants seek to extend the life of their aging components through weld repairs. Some of the repairs require stress relieving using post weld heat treatment (PWHT). However, PWHT is a cost and time consuming process. This paper provides a brief description of different alternative techniques for PWHT: half-bead welding, temper-bead welding and cold repairs. It presents a short survey about the different repairs techniques with or without the PWHT and their use in refineries and power plants in Kuwait and Australia. Some of these repairs now have had a successful life of over a decade; the oldest is nearly 20 years old. Details of the methods used are described and recommendations made concerning the alternative techniques. The availability of skilled labour turns out to be a decisive issue.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.