Abstract

Abstract In pressurized water reactors (PWR), dissimilar metal welds are made to join the pressure vessels of low-alloy steel to pipes of stainless steel using Alloy 182 (UNS W86182) as a filler metal. However, it has been found that Alloy 182 is susceptible to intergranular environmentally assisted cracking (IGEAC) at high temperatures, and this has been one of the major concerns in the management and prediction of plant life. Variation within welds and welders are expected; for design and integrity assessment of the dissimilar welds, these variations should be evaluated. In this study, three dissimilar welds blocks of ASTM A508 steel were prepared using gas tungsten arc welding (GTAW; buttering) and shield metal arc welding (SMAW) processes using Alloys 82/182 (UNS N06082/UNS W86182) as filler metal. Three different welding conditions or heat inputs were used: normal or conventional for the procedure, higher, and normal but cooled. Samples were taken from the three blocks and tested with slow strain rat...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.