Abstract
Austenitic stainless steel has been used as a corrosion resistance material in tough corrosive circumstance. However, austenitic stainless steel has poor wear resistance property due to its low hardness. Tungsten Carbide alloys (WC) are widely used as tooling materials, because of their high hardness and excellent wear resistance property. In this investigation, we apply powder composite process to obtain hard layer of Stainless steel. The composite material was fabricated from planetary ball milled WC powder and SUS316L stainless steel powder and sintered by Pulsed Current Sintering (PCS) method. We also added TiC powder as a hard particle in WC layer. Evaluations of wear properties were performed by pin-on-disk wear testing machine, and a remarkable improvement in wear resistance property was obtained. The weight loss rate of the composite was 1/10 of SUS316L. In addition, it was found that TiC hard particle addition has a positive effect on the wear resistance property. EPMA investigation showed good dispersion of WC hard phase and TiC hard particle with SUS316L matrix.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.