Abstract The wear resistance and Janka hardness of five United States hardwood species were evaluated for potential use in bridge decking and truck flooring. The species tested include ash (Fraxinus sp.), hickory (Carya sp.), red oak (Quercus sp.), sweetgum (Liquidambar styraciflua), and white oak (Quercus sp.). The specimens were prepared with the sizes of 1 by 2 by 4 inches (2.54 by 5.08 by 10.16cm) for abrasion test and 1 by 2 by 6 inches (2.54 by 5.08 by 15.24 cm) for Janka hardness testing. The specimens were cut from 30 individual parent boards of random width with clear sections for each species. The abrasion and Janka hardness tests were performed according to the American Society of Testing and Materials standards. All wear and hardness data were statistically analyzed by 1-way analysis of variance. The results of this study demonstrated that sweetgum with the lowest density had the greatest amount of thicknesses loss and thus lowest wear resistance. White oak was found to have the least thicknesses loss, thus highest wear resistance among the hardwood species tested. Hickory, with the highest density, had the highest hardness among the hardwood species tested, but it had relatively lower wear resistance comparing to ash, red oak, and white oak.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.