Abstract

A map describing the flank wear characteristics of uncoated high-speed steel (HSS) tools is constructed under the condition of drilling die-cast aluminum alloy. Several wear mechanisms are revealed which describe different wear modes observed by SEM in uncoated HSS tools, including adhesive wear, adhesive and abrasive wear, abrasive wear, severely plastic flow, and thermal wear. In the map, there exists a minor wear region, which is called “safety cutting zone” to the HSS tools. This map will be a good reference for choosing suitable drilling parameters of uncoated HSS cutting tools.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.