Abstract

A wear mechanism map of uncoated high-speed steel (HSS) tools was constructed under the conditions of dry-drilling die-cast magnesium alloys. Three wear mechanisms appear in the map based on the microanalysis of drilled HSS tools by SEM, including adhesive wear, abrasive wear and diffusion wear. In the map, there exists a minor wear region which is called “safety zone”. This wear mechanism map will be a good reference for choosing suitable drilling parameters when drilling die-cast magnesium alloys.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.