Abstract

Wear behavior of self-mated stainless steels in NaCl solution has been investigated. The experiment was done in the corrosive liquid of which NaCl concentration of and temperature of . Two kinds of wear type were observed: one is 'severe wear' type which shows gradually increasing wear volume with increasing sliding distances, the other is 'mild wear' type which shows change of wear rate from high value to low at transition distance. The specific wear rate in severe wear type was not sensitive to the liquid temperature and concentration of NaCl but stable at value of approximately.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.