This work investigates the factors affecting the morphology of WC powder. WO3–C mixtures were prepared by high-energy ball milling and nano-sized WC powder was obtained in the form of platelets with a high aspect ratio (5–20) carbothermally. We observed that the WC powder contains excess (101) plane along with high level of strain during initial heating stage. Further, the temperature for the platelet formation coincides with that for the reduction of (101) peak intensity in the XRD pattern. From this study we found that the presence of excess (101) plane and high strain promoted the formation of platelet WC effectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.