Abstract

AbstractThe objective of the study was to investigate the water vapour sorption behaviour of thermally modified (TM) wood powder, e.g. ground wood prepared from waste streams of TM solid wood, and wood powder that was extracted in pressurised hot water. Solid spruce wood was TM in steam conditions (210°C for 3 h), milled and hot-water-extracted (HWE) at elevated pressure (140°C for 1 h). The results evidence that the hot-water extraction reduced the water sorption and the accessible hydroxyl group concentration by the removal of amorphous carbohydrates. In contrast, the enhanced cross-linking of the cell wall matrix and the annealing of amorphous matrix polymers during thermal modification reduced the sorption behaviour of wood additionally, without further reducing the hydroxyl accessibility. These additional effects of thermal modification were at least partially cancelled by hot-water extraction. The results bring novel insights into the mechanisms that reduce the water vapour sorption of wood by compositional and structural changes induced by heating.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.