Abstract
The permeability of small textile samples to water vapor has been evaluated using a conventional DSC cell. The technique enables evaporative rate data to be determined and comparisons made of materials having different characteristics. The data are useful in predicting evaporative sweat loss rates, thereby helping to evaluate metabolic heat loss problems associated with protective clothing for firefighters.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.