Water-soluble substance is an important part of non-rubber substance in natural rubber latex and it has significant influence on the properties of natural rubber. The aim of this paper is mainly to study the composition of small-molecular-weight water-soluble substance (s-WSS) and its effects on the properties of natural rubber films. The analysis of IR and HPLC-MS showed that s-WSS (not including sugar) is composed of C3H4N4O6, C7H14O6, C11H13N3O5, C11H20O7 and C6H22N8. While the main component of s-WSS is C7H14O6 whichis a kind of alcohol. The tensile strength of the prepared composites can be increased at low loading of s-WSS. The tear strength of the prepared composites can be improved by adding s-WSS into natural rubber. The thermal oxidation degradation process of the samples has two stages. Compared with neat natural rubber latex, the initial degradation temperature was decreased significantly in both stages when s-WSS was added. While the degradation temperature range became larger in both stages.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.