Abstract

In an attempt to develop a soybean-protein wood adhesive with improved water resistance and good technical applicability, soybean protein was first degraded under strong alkali conditions and then subjected to chemical crosslinking combined with nano-modification. Results of plywood evaluation, GPC analysis, and XRD determination indicated that a soybean-protein adhesive that could bear 28 h boiling-dry cycled treatment according to standard JIS K6806-2003. The water-resistance improvement was attributed to both the chemical crosslinking of the degraded soybean protein (DSP) by MDI and the nano-modification of DSP by intercalated or exfoliated montmorillonite (MMT). Caustic degradation improved the technical applicability of the DSP adhesive by sharply reducing the viscosity of high-content protein solution. MMT nano-modification can obviously prolong the pot lives of MDI-modified DSP adhesives but slightly decrease their dry bond strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.