Abstract

Technology is developed for two-stage processing of secondary zirconium-containing mineral resource. A production scheme includes mechanical treatment of bacor waste and subsequent chemical leaching of impurities. The main processes in the first (mechanical) stage are crushing and selective grinding with separation of high-zircon concentrate (Al2O3–ZrO2 system) and aluminum-zirconia product leaner with respect to ZrO2 (R 2O–Al2O3–ZrO2–SiO2 system). In the second stage the latter are leached with a fluoric acid solution. The waste-free technology proposed for enrichment makes it possible to use valuable secondary resources entirely with preparation of two end products: enriched bacor refractory and a slag-forming mixture for steel smelting production.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.