Molybdenum disulfide (MoS2) thin films were grown directly on SiO2 covered wafers by atomic layer deposition (ALD) at the deposition temperatures ranging from 175 to 225°C using molybdenum hexacarbonyl [Mo(CO)6] and H2S plasma as the precursor and reactant, respectively. Self-limited film growth on the thermally-grown SiO2 substrate was observed with both the precursor and reactant pulsing time. The growth rate was ∼0.05nm/cycle and a short incubation cycle of around 13 was observed at a deposition temperature of 175°C. The MoS2 films formed nanocrystalline microstructure with a hexagonal crystal system (2H-MoS2), which was confirmed by X-ray diffraction and transmission electron microscopy. Single crystal MoS2 nanosheets, ∼20nm in size, were fabricated by controlling the number of ALD cycles. The ALD-MoS2 thin films exhibited good stoichiometry with negligible C impurities, approximately 0.1at.% from Rutherford backscattering spectrometry (RBS). X-ray photoelectron spectroscopy confirmed the formation of chemical bonding from MoS2. The step coverage of ALD-MoS2 was approximately 75% at a 100nm sized trench. Overall, the ALD-MoS2 process made uniform deposition possible on the wafer-scale (4in. in diameter).
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.