High-quality (Gd0.955−xZn0.045)PO4:xTb3+ (0.06≤x≤0.15) green phosphors were synthesized by ultrasonic spray pyrolysis. With an increase of Tb3+ content, the emission intensities caused by the 5D4→7FJ (J = 3, 4, 5, and 6) and 5D3→7FJ (J = 4, 5, and 6) transitions of Tb3+ increased and decreased, respectively, allowing a purer green emission. The emission intensity of (Gd0.805Zn0.045)PO4:0.15Tb3+ at 544 nm was 53.0% stronger than that of (Gd0.895Zn0.045)PO4:0.06Tb3+. The emission intensity and the green color purity were remarkably improved by increasing Tb3+ content in (Gd0.955−xZn0.045)PO4:xTb3+.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.