Composites with BQTN 157-EX polyester matrix Yukalac reinforced with bambusablumeanafiber and glass fiber are used to find the right reinforcement composition. For natural fibers that are used to get special treatment, namely the separation of fibers by alkaline immersion process. The mixing process of the 2%, 2.5% and 3% reinforcement volume fraction was used for ASTM D638M-84 tensile testing variations. The maximum tensile strength is obtained in the bamboo powder and glass fiber fraction with a length of 5 mm with a value of 53.581 MPa. Void observations in the form of bubbles were carried out by quantitative metallographic analysis of ASTM E112-10 standards. The result of macroscopic enlargement, most voids in the volume fraction of reinforcement 3% of bamboo fiberhaur and glass 5 mm long an average of 9 point grid. The greater the volume volume fraction of the mixed bamboo and fiberglass, increasing the likelihood of voids occurring.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.