Abstract

This study investigated an effect of different ways of the preparation of insoluble hyaluronan material on its mechanical and viscoelastic properties. Hyaluronan (NaHy) of molecular weight Mw=500,000 g mol(-1) was modified with N-(3-dimethylaminopropyl-N'-ethylcarbodiimide hydrochloride (EDC) and N-hydroxysuccinimide (NHS), to be able absorb liquid without changing its mechanical properties. The modified, water insoluble NaHy materials were prepared in different geometry; as modified films and modified cylinders with exact dimensions. The occurrence of modification was confirmed by FT-IR (Fourier transform infrared spectroscopy) and (1)H NMR (proton nuclear magnetic resonance) spectroscopy and swelling test. The determined mechanical and viscoelastic properties of unmodified and modified hyaluronan revealed the high dependency of elasticity changes depending on the gel processing method. Moreover, NaHy gels in the cylindrical form with the sponge-like structure predominant them as a convenient geometry for application in a humid environment.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.