Abstract

Current-induced domain-wall motion experiments in 27nm thick and 200–500nm wide Fe20Ni80 wires are reported. By imaging the domain-wall position after current injections, the mean wall velocities are determined. The initial velocity is found to be constant for pulse lengths between 2 and 25μs but decays after about ten injections. For samples with an increasing wire width the initial velocity is reduced.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.