Abstract
Subnanoporosity was introduced into SiOCH-based thin films by mixing tetraethyl orthosilicate with hexamethyldisiloxane (HMDSO) in the plasma enhanced chemical vapor deposition process, and was evaluated by the variable-energy positron annihilation lifetime technique. It was found that with increasing the HMDSO fraction both porosity and pore size were enhanced, as evidenced by the decreased refractive index and increased ortho-positronium lifetime. The lifetimes from 2.0 to 6.8 ns suggested the tunable pore volumes within a range of 0.1–0.7 nm 3.