Abstract

A simple and facile vapor-assisted hydrolysis route has been used to synthesize Al2O3-coated LiCoO2. The effects of Al2O3 coating on the structure and electrochemical performance have been systematically studied. After deposition of the Al2O3 coating, the crystal structure and morphology of LiCoO2 are maintained. Galvanostatic charge-discharge tests show that Al2O3-coated LiCoO2 exhibits markedly improved capacity retention and rate capability at high charge voltage (4.5V). The Al2O3-coated LiCoO2 exhibits an initial discharge capacity of 165.5mAh/g at 360mA/g, and the capacity retention is 98.6% after 180 cycles. The electrochemical impedance spectroscopy results demonstrate that the Al2O3 coating can slow the increase of charge-transfer resistance during cycling, which is in accord with the excellent electrochemical cycling performance of Al2O3-coated LiCoO2.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.