Abstract

The Y3Al5−xGaxO12(YAGG):Ce3+-Cr3+ persistent phosphor is one of the materials in which Cr3+ ions act as electron traps. The possibility of electron traps by other transition metal ions (TM3+, TM = Sc, Ti, V, Cr, Fe) was investigated and those electron trap depth was compared with each other. In the thermoluminescence (TL) glow curves, the YAGG:Ce3+ samples co-doped with different TM3+ ions show different TL glow peak temperatures (i.e. different electron trap depth). The estimated vacuum referred binding energy of TM2+ from the trap depth shows a zig-zag curve, which is found to be originated from the different 3d electron energies affected by a number of d electron, nuclear charge and crystal field splitting. Utilizing the obtained TM2+ zig-zag curve, a new persistent phosphor of Y3Al2Ga3O12:Ce3+-Sc3+ and a photostimulated phosphor of Y3Al2Ga3O12:Ce3+-V3+ were successfully developed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.