Abstract

As a substitute for fried clay and stone powder-cement bricks, this study developed novel green bricks based on coal-combustion bottom ash (CCBA) obtained from a thermal power plant in Vietnam. By using varied replacement amounts of stone powder at 0, 10, 20, 30, and 40% in weight, ten brick compositions with water-to-binder (w/b) ratios of 0.35 and 0.40 were developed. Testing was done on the bricks' characteristics, such as compressive strength, ultrasonic pulse velocity, water absorption, water permeability, electrical resistance, and thermal conductivity. The findings showed that increasing CCBA content or w/b ratio has a negative impact on the characteristics of unburnt bricks. However, all the brick samples made for this investigation performed exceptionally well when compared to the requirements of the national Vietnamese standard. The brick samples produced in this study are recommended to apply in real practice.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.