Abstract

The paper analyses the possibilities of recycling tannery sludge (TS) in clay brick manufacture. The physico-mechanical properties and microstructure of clay brick and cement mortars vary depending on TS content in the mix. 2.5 % 15.0 . TS (by weight) was added to clay bricks fired at 1000 .C temperature and maintained at maximum heat for 1 hour. The tests revealed that 2.5 . TS addition had a positive effect on physical and mechanical properties of clay brick: reduce drying and firing shrinkage, reduce water absorption, and increase compressive strength. Chromium leaching values in clay brick (2.5 % TS) were found not to exceed the limit values set forth in 2003/33/EC.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.