Abstract

The purpose of this study was to use a new scratch test and tensile test to evaluate the bond strength between artificial erosive enamel or dentin and self-adhesive resin composites as a coating material. Coronal enamel or dentin surface was exposed to an erosive cycle (artificial saliva [AS], pH:7.0 for 6.5 h and acidic carbonated beverages for 5 min, alternated 3 times per day) for the eroded-surface or stored in AS for the remineralized-surface. Two self-adhesive flowable resin composites, Fusio and LLB-CR6 (prototype), and a conventional flowable resin composite, BEAUTIFIL FLOW with self-etching primer system, Clearfil Mega Bond, were applied to enamel or dentin surfaces; and then the bond strengths were measured. For the eroded-surface, there were no significant differences in bonding strength among all materials, as assessed by the new scratch test. Thus, these self-adhesive flowable resin composites might be useful for coating materials on acid-eroded tooth surfaces.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call