Abstract

The present study investigated the effect of 2-isocyanatoethyl methacrylate (IEM) and iron (II) perchlorate on dentin adhesion. Four primers were evaluated, consisting of aqueous 2-hydroxyethyl methacrylate (HEMA) solutions containing 5, 10, 20 or 50 micromol/g iron (II) perchlorate. Five luting agents were prepared with methyl methacrylate (MMA), poly(methyl methacrylate) (PMMA), tri-n-butylborane (TBB) initiator and IEM. The concentrations of IEM in the luting agents were 0.2, 0.4, 0.8, 2.0 and 4.0 wt%. Extracted bovine teeth were ground to expose the dentin, etched with an aqueous solution of 10 wt% phosphoric acid, primed, and then bonded with stainless-steel rods; tensile bond strengths were determined after 1 d immersion in water. The highest bond strength (20.7 MPa) was recorded for the group using 10 micromol/g iron (II) perchlorate and 2.0 wt% IEM. The use of IEM was effective in decreasing the optimal concentration of iron (II) perchlorate, and this may contribute to the color stability of iron-containing pretreatment agents.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.