Abstract

The processing of nickel laterite ore to produce ferronickel is energy intensive, especially when low nickel content ores are processed. The selective reduction–beneficiation of laterite ore to produce high nickel content nickeliferous concentrate and abandon gangue minerals before smelting potentially offers an effective pre-treatment to this process. In this work, the authors conducted selective reduction of nickel laterite ores at 1100°C for 60min with addition of 6% calcium sulfate and 5% reductant coal. The reduced ore was then wet magnetic separated. The experiments show that high nickel content nickeliferous concentrate containing 6.0% Ni with nickel recovery of 92.1% could be produced with over 75% of the reduced ore, containing low nickel concentration, rejected. The tests indicated that the selectivity of reduction depends mainly on reduction atmosphere and silica level. According to the microscopic study, nickel oxide had been reduced and nickel was mainly enriched into a γ Fe–Ni phase. The presence of sulfur significantly promoted γ Fe–Ni particle growth, from 5.8μm to 16.1μm, and improved the Ni enrichment in metallic phases.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.