Abstract

A gradual upgrade of refractory lining of 160-ton teeming ladles, the disadvantages of the previous lining schemes, and methods for their elimination are described. The implementation of developed techniques has increased the resistance of teeming ladle lining by 60% (from 50 to 80 heats) and the consumption of refractory in the working layer of lining has decreased by 35.7% (from 4.79 to 3.08 kg/t of steel.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.