Abstract

Aldol condensation of furfural with acetone (molar ratio 1:10) was carried out in a flow fixed bed setup at 50°C using calcined hydrotalcite with Mg/Al of 3 as a catalyst. Complete conversion of furfural and stable catalyst performance was obtained during the initial 50h on stream. This period was followed by a rapid catalyst deactivation. In contrast to previous reports, higher molecular weight products that were identified as products of successive aldol condensation of acetone with furfural were observed. Their concentration was time-dependent with a maximum formation after 10 to 30h on stream.

Full Text
Published version (Free)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call