Abstract

An investigation was conducted to establish the effects of specimen preparation and configuration on the measured compressive strength of unidirectional carbon fibre. The compressive strength was determined through ASTM D 695 M [ASTM D 695 M, Standard test method for compressive properties of rigid plastics. http://www.astm.org] test method. Specimens conforming to this standard were produced with different thickness, edge and surface preparation. Optical and electron (SEM) microscopical techniques were used to assess initiation of failure and to quantify the damage encountered by the compressive test specimen. The findings correlated well with the mechanical test results, additionally; from the mechanical testing there was significant evidence to suggest that the failure mechanism is dependent upon the quality of the preparation of the test specimen.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.