Abstract

The lithium-ion transport mechanism in 0.7Li(CB9H10)-0.3Li(CB11H12) complex hydride solid electrolyte was studied over a wide time-scale (ns-ms) by choosing appropriate techniques for assessing ionic motion on the desired time-scale using nuclear magnetic resonance (NMR) relaxation, AC impedance, and pulsed field gradient-NMR (PFG-NMR) measurements. The 7Li NMR line width decreased with increasing temperature, and the spin-lattice relaxation time T1 for the cation and anions showed a minimum near 303 K, indicating that the lithium ions and the anions were highly mobile. The activation energy estimated from the analysis of the NMR relaxation time matched well with the values estimated from the AC impedance and PFG-NMR. This confirms that the lithium-ion motion in 0.7Li(CB9H10)-0.3Li(CB11H12) is the same over a wide time-scale, suggesting steady Li-ion motion over a wide transport range. This understanding offers insights into strategies for designing complex hydride lithium superionic conductors.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.