Abstract

Ultraviolet-ozone (UV-O3) treatment is a simple but effective technique for surface cleaning, surface sterilization, doping, and oxidation, and is applicable to a wide range of materials. In this study, we investigated how UV-O3 treatment affects the optical and electrical properties of molybdenum disulfide (MoS2), with and without the presence of a dielectric substrate. We performed detailed photoluminescence (PL) measurements on 1–7 layers of MoS2 with up to 8 min of UV-O3 exposure. Density functional theory (DFT) calculations were carried out to provide insight into oxygen-MoS2 interaction mechanisms. Our results showed that the influence of UV-O3 treatment on PL depends on whether the substrate is present, as well as the number of layers. Additionally, 4 min of UV-O3 treatment was found to be optimal to produce p-type MoS2, while maintaining above 80% of the PL intensity and the emission wavelength, compared to pristine flakes (intrinsically n-type). UV-O3 treatment for more than 6 min not only caused a reduction in the electron density but also deteriorated the hole-dominated transport. It is revealed that the substrate plays a critical role in the manipulation of the electrical and optical properties of MoS2, which should be considered in future device fabrication and applications.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.